Low Density Closed Cell Red Heat Insulation Silicone Foam Sponge Tube
1). Non-toxic, odorless, transparent, flame retardant, non-yellowing 2). Soft, flexible, kink resistance to deformation 3). Not cracking, durable, resistant to high and cold temperature 4). High tear strength and superior electrical performance 5). Various sizes, colors, durometer could be available 6).Oil,heat,low-temperature,ozone/UV resistant
Description
- Closed cell silicone foam tube are widely used in door, window and high temperature machines industry.
- Closed cell silicone sponge tube are extruded products which are made of special silicone raw material, adding some proportion of foam auxiliary material to form the shape of sponge honeycomb.
- Hollow silicone foam tube are called foam silicone hose, sponge silicone tube, heat retaining silicone tube or heat insulation silicone tube.
- Red silicone foam tube have excellent properties of heat resistance, ozone resistance, insulation, permanent compression set value, elasticity and sealing.
- Low density silicone sponge tube are usually used in the parts of heat preserving, heat shielding, damping,noise reducing, waterproof sealing and weight reducing.
Specifications
- Non-toxic, odorless, transparent, flame retardant, non-yellowing
- Soft, flexible, kink resistance to deformation
- Not cracking, durable, resistant to high and cold temperature
- High tear strength and superior electrical performance
- Various sizes, colors, durometer could be available
- Oil,heat,low-temperature,ozone/UV resistant
| Application: | Protecting silicone foam tube |
| Material: | Sponge Silicone,EPDM or PVC,with steel insert or not,in different color choices |
| Production method: | Extrusion and cut |
| Color | Any color you need |
| Packing: | By rolls |
| Certification: | ISO 9001:2008 |
| Dimensions: | As per customer's drawings or samples |
Technical Parameters:
| Material: | Special Silicone, Foam auxiliary |
| Color: | Customized |
| Hardness (shore C): | 15°~70°±5° |
| Density (g/cm3): | 0.2~1.0±0.1 |
| Tearing Strength(KN/m): | ≥2 |
| Tensile Strength(Mpa): | ≥0.8 |
| Elongation at Break %: | ≥200 |
| Working Temperature (℃): | -40~200° |
| Smell: | Slight |
| Flammability (UL-94): | HB~V-0 |
| Thermal Conductivity W/m.k: | ≤0.1 |
| Permanent Compression Set Value 25%: | ≤12 |
| Grade: | ROHS |
|
|
|
|
|
|